| 14X17H2 |
It has higher chromium grade of the nickel-bearing, hardenable, stainless steel by high mechanical properties.
Composition:
| %C | %Si | %Mn | %P | %S | Cr | Ni | Ti | Cu |
| 0.11-0.17 | Max0.8 | Max0.8 | Max0.03 | Max0.025 | 16-18 | 1.5-2.5 | Max0.2 | Max0.3 |
Hot working:
Forging temperature range: 1230-850℃
Note: Heat to 1230 ℃. Do not forge below 850.
Heat treatment:
| annealing ℃ | Normalizing ℃ | Hardening temperature for quenching in Water ℃ |
| Full annealing is not recommended. Recommended temperature for annealing is 620-705 | Don’t normalize | 980 |
Main application:
High strength mechanical engineering components
Shape of product:
Round, flat, step shape, ring, disc, shaft, other shape depend on customer needs